A wood shrinkage calculator predicts how much a board changes in width when its moisture content changes. Wood swells when it takes up moisture and shrinks when it dries, and it moves most across the grain. Pick the species, say whether the board is plainsawn or quartersawn, enter its width and the starting and ending moisture content, and the tool gives the change in width and the new width. It uses the average shrinkage values of the US Forest Products Laboratory [1].
How to use the wood shrinkage calculator
- Choose US (inches) or Metric (millimetres).
- Pick the species of wood.
- Choose tangential for plainsawn boards or radial for quartersawn boards.
- Enter the width of the board.
- Enter the starting moisture content and the ending moisture content, in percent.
- Leave the fibre saturation point at 30 percent unless you know it, then press Calculate.
Why wood moves
Shrinkage begins at the fibre saturation point, which averages about 30 percent moisture content, and continues in a fairly linear way until the wood is completely dry [1]. Above that point the cell walls are full and the wood does not change size. The movement differs by direction. Tangential shrinkage, along the growth rings, is about twice as great as radial shrinkage, across them [1]. Lengthwise movement is small, usually between 0.1 and 0.2 percent from green to ovendry for most species [1], so this tool covers width and thickness only.
The formula
The Handbook assumes that shrinkage begins at the fibre saturation point and that dimensions decrease linearly as moisture content falls. Its table gives the shrinkage S0 from green to ovendry as a percentage of the green dimension [1]. From those assumptions, our own working is:
- Shrinkage at moisture content x, as a percent of the green size: S(x) = S0 × (fibre saturation − x) ÷ fibre saturation, and 0 at or above the fibre saturation point.
- New size = old size × (1 − S(end) ÷ 100) ÷ (1 − S(start) ÷ 100).
- Change = new size − old size.
A negative change means the board shrinks, a positive change means it swells.
Which value applies: tangential or radial?
The Handbook says to use tangential values for the width shrinkage of plainsawn material and radial values for quartersawn material. For mixed or unknown ring orientation it suggests tangential values [1]. The tool defaults to tangential.
Shrinkage values used (green to ovendry)
| Species | Radial (%) | Tangential (%) |
|---|---|---|
| White oak | 5.6 | 10.5 |
| Northern red oak | 4.0 | 8.6 |
| Sugar maple | 4.8 | 9.9 |
| Red maple | 4.0 | 8.2 |
| Black cherry | 3.7 | 7.1 |
| Shagbark hickory | 7.0 | 10.5 |
| Yellow-poplar | 4.6 | 8.2 |
| White ash | 4.9 | 7.8 |
| Eastern white pine | 2.1 | 6.1 |
| Loblolly pine | 4.8 | 7.4 |
| Ponderosa pine | 3.9 | 6.2 |
| Douglas-fir (coast) | 4.8 | 7.6 |
| Western redcedar | 2.4 | 5.0 |
| Redwood (old growth) | 2.6 | 4.4 |
Worked example
A plainsawn white oak board is 10 inches wide at 12 percent moisture and dries to 6 percent. The tangential value is 10.5 percent. At 12 percent the shrinkage from green is 10.5 × (30 − 12) ÷ 30 = 6.3 percent. At 6 percent it is 10.5 × 24 ÷ 30 = 8.4 percent. The new width is 10 × (1 − 0.084) ÷ (1 − 0.063) = 9.776 inches, so the board shrinks by 0.224 inch, or 2.24 percent.
If the same board were quartersawn the radial value 5.6 percent applies, and it would shrink only 0.116 inch. An eastern white pine board of the same size, plainsawn, shrinks 0.127 inch because pine moves less than oak. A board that dries from 30 percent to 8 percent loses 7.7 percent of its width, or 0.77 inch on a 10 inch board.
Practical advice
- Let wood reach the humidity of the room before you build. A board that has equalised with the room moves much less.
- Leave room for movement. A wide panel glued tight across its width can crack when it dries.
- Narrow boards move less than wide ones. Several narrow boards in a panel spread the movement over more joints.
- Quartersawn boards move about half as much in width as plainsawn boards, which is why they are used for stable work.
- In a heated house in winter the air is dry and wood shrinks. In a humid summer it swells again.
Accuracy and limits
These are averages. The Handbook says the shrinkage of individual pieces varies and that the variation can be described by a coefficient of variation of about 15 percent [1]. A prediction of 0.22 inch should therefore be read as roughly 0.19 to 0.26 inch. The linear model also ignores moisture gradients inside thick boards, which shrink before they are dry at the centre.
Only the species in the list are included. For a species not listed, pick a similar one and expect error. Warping, cupping and twisting are not predicted.
Using the result in a project
Take the change in width and decide where it goes. For a tabletop built at 12 percent moisture and kept in a home that averages 7 percent in winter, enter those two figures and read the shrinkage across the top. Then leave at least that much room, for example with slotted screw holes or table-top fasteners that let the top slide. For flooring, the same figure tells you the expansion gap to leave at the walls. For a door panel, it tells you how much clearance to give the frame so the panel does not bind in summer.
Common mistakes
- Using the green to ovendry percentage for a small change. Use the start and end moisture instead, as this tool does.
- Entering a moisture content above 30 percent. The tool treats everything above the fibre saturation point as no change.
- Mixing up radial and tangential values.
- Expecting the answer to match a single board exactly.
What next
Use this often? Add Wood Shrinka to your Home screen.
Frequently asked questions
How does a wood shrinkage calculator work?
It takes the average shrinkage of the species from green to ovendry, assumes shrinkage begins at the fibre saturation point and is linear below it, and applies that to the moisture change you enter.
How much will a 10 inch oak board shrink?
A plainsawn white oak board that dries from 12 to 6 percent moisture content shrinks about 0.22 inch. A quartersawn one shrinks about 0.12 inch.
Does wood shrink in length?
Very little. Lengthwise shrinkage from green to ovendry is generally 0.1 to 0.2 percent, so width and thickness are what matter.
What is the fibre saturation point?
It is the moisture content at which the cell walls are full of bound water. It averages about 30 percent, and wood only shrinks below it.
Is plainsawn or quartersawn wood more stable?
Quartersawn. Tangential shrinkage is about twice the radial value, so quartersawn boards move roughly half as much in width.
Was this tool helpful?
What went wrong?
We only receive the reason you pick, never what you typed into the tool.
Thanks for your feedback.