Use this welding calculator to work out heat input and arc energy from voltage, current and travel speed, with process efficiency for MIG, stick, flux-cored, TIG and submerged arc.

Restored your last values ·

Take the voltage and current from the machine or a meter while welding. Travel speed is how fast the torch or electrode moves along the joint.

Everything is worked out in your browser. Nothing you type is sent anywhere.

Heat input

–

Enter the process, voltage, current and travel speed, then press Calculate.

See full result

This welding calculator works out the heat input and arc energy of an arc weld from the voltage, current and travel speed. Choose the welding process, enter the arc voltage and current and the travel speed (or a weld length and the time it took), and the welding calculator gives the heat input in kJ per inch or kJ per millimeter, the arc energy and the total heat for the weld.

How to use the welding calculator

  1. Choose US or metric units. US (inches per minute and kJ per inch) is the default.
  2. Choose the welding process.
  3. Enter the arc voltage and welding current.
  4. Enter the travel speed, or the weld length and arc time to work it out, then press Calculate.

Heat input and arc energy

TWI, the welding research organization, explains that heat input and arc energy are both measures of how much energy is supplied to the workpiece to form a weld, measured as energy per unit length: kJ/mm in Europe and kJ/in in America. Arc energy is the energy supplied by the arc before the process efficiency is considered:

arc energy = (voltage × current × 60) ÷ (1,000 × travel speed)

With voltage in volts, current in amps and travel speed in inches or millimeters per minute, this gives kJ/in or kJ/mm. The 60 turns minutes into seconds, and dividing by 1,000 turns joules into kilojoules. Heat input, which TWI calls the present best-practice term, accounts for how much of that energy actually reaches the workpiece: heat input = η × arc energy, where η is the process efficiency.

Process efficiency factors

Each arc welding process has a different efficiency. TWI gives these factors, all relative to submerged arc welding:

ProcessEfficiency factor η
Submerged arc welding (SAW)1.0
Manual metal arc / shielded metal arc (MMA/SMAW, stick)0.8
Flux-cored arc welding (FCAW)0.8
Metal inert/active gas (MIG/MAG, GMAW)0.8
Tungsten inert gas (TIG, GTAW)0.6
Plasma arc welding0.6

TWI notes that a number of American codes use the term heat input when they mean arc energy, without the efficiency factor. The calculator shows both, so you can use whichever your code requires.

Worked example

A MIG (GMAW) weld runs at 24 volts and 200 amps with a travel speed of 12 inches per minute. The arc energy is 24 × 200 × 60 ÷ (1,000 × 12) = 24 kJ/in. With GMAW's efficiency of 0.8, the heat input is 19.2 kJ/in, about 0.76 kJ/mm. A TIG weld at 12 volts, 120 amps and 4 inches per minute has an arc energy of 21.6 kJ/in and a heat input of 12.96 kJ/in.

In metric, a weld at 25 volts, 180 amps and 300 mm per minute has an arc energy of 0.9 kJ/mm; as a GMAW weld, its heat input is 0.72 kJ/mm.

Measuring travel speed

If you don't know the travel speed, weld a measured length and time the arc. The calculator divides the length by the time to get the speed. For example, a 6-inch weld that takes 30 seconds is 12 inches per minute. It also multiplies the heat input by the length to give the total heat put into that weld.

Reading the results

The big number is the heat input, including the process efficiency. The table shows the arc energy before efficiency, the efficiency factor used, the heat input in the other unit, the travel speed and, if you entered a weld length, the total heat in kilojoules.

Why heat input matters

Heat input affects how quickly a weld and the metal around it cool, which in turn affects the weld's strength and toughness and the risk of distortion. The Wikipedia article on arc welding notes that in arc welding the voltage is directly related to the length of the arc, and the current is related to the amount of heat input. Welding procedures often set a range of heat input, so welders can check their settings stay within it.

Converting between kJ/in and kJ/mm

Because there are 25.4 millimeters in an inch, a heat input in kJ per inch is divided by 25.4 to give kJ per millimeter, and a figure in kJ per millimeter is multiplied by 25.4 to give kJ per inch. The calculator shows both, whichever units you choose, so you can compare your settings with a procedure written in either system. For example, 19.2 kJ/in is about 0.756 kJ/mm, and 0.72 kJ/mm is about 18.3 kJ/in.

How each setting changes the result

The formula shows how each setting affects the energy put into the joint. Raising the voltage or the current raises the arc energy in the same proportion: at the same speed, 10% more current gives 10% more energy per inch. Travel speed works the other way. Doubling the speed halves the energy per inch, because the same power is spread over twice the length of weld. Slowing down, or weaving the torch so it moves forward more slowly, puts more energy into each inch.

Total heat for a weld

If you enter a weld length and arc time, the calculator also multiplies the heat input by the length to give the total energy for that weld. A 6-inch submerged arc weld at 24 volts, 200 amps and 12 inches per minute has a heat input of 24 kJ/in, so the whole weld takes about 144 kJ. This can be useful when comparing two ways of making the same joint, such as one large pass against several smaller ones.

Common mistakes

  • Mixing up definitions. Some codes use arc energy, others heat input with η.
  • Using set values instead of actual ones. Measure voltage and current while welding.
  • Timing weave or pauses wrongly. Use the arc-on time for the length welded.
  • Mixing units. Inches per minute give kJ/in; millimeters per minute give kJ/mm.

Tips

  • Record voltage, current and speed for each pass.
  • Keep heat input within your procedure's range.
  • Use the same method each time so results are comparable.

What next

Use this often? Add Welding to your Home screen.

Frequently asked questions

How does a welding calculator work?

It works out arc energy = V × I × 60 ÷ (1,000 × travel speed) and multiplies it by the process efficiency to give heat input.

How do you calculate welding heat input?

Heat input = η × (volts × amps × 60) ÷ (1,000 × travel speed).

What is the efficiency factor for MIG welding?

TWI gives 0.8 for MIG/MAG (GMAW), 0.6 for TIG and 1.0 for submerged arc.

What is the difference between heat input and arc energy?

Arc energy is the energy from the arc; heat input multiplies it by the process efficiency, although many American codes use heat input to mean arc energy.

What is the heat input at 24 V, 200 A and 12 in/min?

Arc energy 24 kJ/in; for GMAW, heat input 19.2 kJ/in.

What went wrong?

We only receive the reason you pick, never what you typed into the tool.

Thanks for your feedback.

More Physics & Science Tools