A Brinell hardness calculator finds the Brinell hardness number of a metal from the diameter of the indentation that a hardened ball leaves in it. It uses the standard 10 millimetre ball and 3,000 kilogram-force load unless you change them, and it gives the hardness in megapascals and an approximate tensile strength.
How to use the Brinell hardness calculator
- Enter the diameter of the indentation.
- Change the load and the ball diameter if the test was not 10/3000.
- Press Calculate.
The test
In the Brinell test, a hard ball is pressed into the surface of a metal with a known load, and the diameter of the indentation is measured. The page says that the standard test uses a 10 millimetre ball and a load of 3,000 kilograms-force, which is about 29,420 newtons [1]. A softer metal gives a larger indentation and so a lower hardness number.
The formula
The page gives the hardness, written HBW, with F the load in newtons, D the diameter of the ball and d the diameter of the indentation, in millimetres [1]. It uses a constant of 0.1022 to convert newtons to kilograms-force, but the layout of the formula is garbled in the text that we could read. The calculator therefore uses the standard form HBW = 2P ÷ [π D (D − √(D² − d²))], with P in kilograms-force, which is the same relation.
A worked example
For the standard 10/3,000 test and an indentation of 4 millimetres, the calculator gives 228.77, which is written as 229 HBW. The page says that indentation diameters usually range between 2.4 and 6 millimetres [1], so 4 millimetres is a typical figure. A diameter of 3 millimetres gives a harder 415 HBW, and 5 millimetres gives a softer 143 HBW. These values are our own calculations.
Load in newtons
If your machine gives the load in newtons, choose that option and the calculator divides by 9.80665 to get kilograms-force. A load of 29,419.95 newtons is 3,000 kilograms-force and gives the same result. The page also lists the other standard loads for a 10 millimetre ball, 1,500 kilograms-force and 1,000 kilograms-force, and for smaller balls [1].
Megapascals
The page says that the Brinell hardness value, expressed as HBW, is multiplied by the acceleration due to gravity, 9.80665 metres per second squared, to convert it to megapascals [1]. For 228.77 HBW, that is 2,243.4 megapascals. The calculator shows both. The units are rarely written with the Brinell number, which is quoted as a plain number such as 250 HB.
Tensile strength
The page notes that the hardness number divided by two gave the approximate ultimate tensile strength of steels in ksi [1]. For 228.77 HBW, this is 114.4 ksi, or 788.7 megapascals. The page adds that the relation depends on the material and has to be found by experiment [1]. Treat the estimate as a guide only, and use a tensile test for any design value.
Checking the indentation
A good indentation is neither too small nor too large compared with the ball. A common rule, which is our own knowledge and not from the page, is that the diameter should be between 24 and 60 percent of the ball diameter, which is 2.4 to 6 millimetres for the 10 millimetre ball. The calculator warns when the diameter is outside this range, and you should then test with a different load.
Standards
The page cites ISO 6506-1 and ASTM E10 for the test [1]. These standards set out how to prepare the surface, the spacing of the indentations, the thickness of the sample and the way to measure the indentation. Follow the current version of the one that applies to your work, and use the calculator only for the arithmetic.
Limits
The Brinell test suits castings, forgings and soft to medium metals. It is not suitable for very hard metals, for which the ball may deform, nor for thin sections or small parts, where another test such as Rockwell or Vickers is used. The calculator does not convert between hardness scales, and the conversions that are in tables are only approximate.
Using the calculator
Measure the diameter of the indentation, in millimetres, with a microscope or a gauge. Enter it. Leave the load and the ball diameter blank for the standard test. Read the hardness number, and the megapascal value. Enter several indentations, one at a time, and average the results, as the standards require, for a reliable hardness.
Hardness of common metals
As a guide, which is our own and should be checked in a handbook, annealed aluminium is around 30 HBW, mild steel in the range of 120 to 150, and hardened tool steel above 500. Cast iron and structural steels lie in between. A hardness of 229 HBW, as in the example, is typical of a medium-carbon steel in the normal condition. Use measured values for your material, since heat treatment changes the figures widely.
Repeat tests
Make at least three indentations, well away from the edges and from each other, and average the hardness numbers that you get. A large scatter shows that the material is not uniform, or that the surface was not prepared well. Enter each diameter in the calculator to compare them.
Common mistakes
- Using the radius instead of the diameter. Enter the diameter.
- Using the wrong load. Check the test condition.
- Trusting the tensile estimate. It is only a rule of thumb.
- Reading very small indentations. They are hard to measure well.
What next
Use this often? Add Brinell Hard to your Home screen.
Frequently asked questions
What is a Brinell hardness calculator?
A tool that finds the Brinell hardness number from the indentation of a ball.
What is the standard Brinell test?
A 10 mm ball with a load of 3,000 kgf, about 29,420 N.
How do I convert HBW to MPa?
Multiply by 9.80665.
What is the range of indentation diameters?
Usually between 2.4 and 6 mm for the standard test.
Can I find tensile strength from hardness?
Roughly: half the hardness number in ksi for steels, but it depends on the material.
Sources
Was this tool helpful?
What went wrong?
We only receive the reason you pick, never what you typed into the tool.
Thanks for your feedback.